Type 244 One Piece Propane/Natural Gas Bulk Head Tip

Type 244 One Piece Propane/Natural Gas Bulk Head Tip

LP Cutting Tips - Type 244

Where To Buy


Features

  • Cutting close to bulk heads
  • Rivet cutting


Industries

  • Industrial and General Fabrication
  • Repair and Maintenance
  • Structural Steel Fabrication
  • Light Fabrication

Specifications

Fuel Specifications

0330-0344

Gas Pressure - Cutting Oxygen 35-40 psig
Gas Pressure - Fuel Gas 3-6 psig
Total Fuel Gas Consumption 22-110 cfh
Total Oxygen Consumption 115-125 cfh
Total Preheat Oxygen Consumption 44-240 cfh
Gas Pressure - Cutting Oxygen 40-45 psig
Gas Pressure - Fuel Gas 4-8 psig
Total Fuel Gas Consumption 22-110 cfh
Total Oxygen Consumption 125-135 cfh
Total Preheat Oxygen Consumption 44-240 cfh

Operating Specifications

0330-0344

Average Kerf Width 0.09 in.
Cutting Speed 14-18 in./min
Metal Thickness 1 in.
Tip Size 2 in.
Average Kerf Width 0.09 in.
Cutting Speed 12-16 in./min
Metal Thickness 1 1/2 in.
Tip Size 2 in.