Specifications

Fuel Specifications

0330-0058

Gas Pressure - Acetylene 3-5 psig
Gas Pressure - Cutting Oxygen 25-30 psig
Gas Pressure - Preheat Oxygen 3-5 psig
Total Acetylene Consumption 5-8 cfh
Total Oxygen Consumption 55-60 cfh
Total Preheat Oxygen Consumption 5-9 cfh
Gas Pressure - Acetylene 3-5 psig
Gas Pressure - Cutting Oxygen 30-35 psig
Gas Pressure - Preheat Oxygen 3-6 psig
Total Acetylene Consumption 6-10 cfh
Total Oxygen Consumption 60-65 cfh
Total Preheat Oxygen Consumption 7-11 cfh

Operating Specifications

0330-0058

Average Kerf Width .06 in.
Cutting Speed 24-28 in./min
Metal Thickness 3/8 in.
Tip Size 0 in.
Average Kerf Width .06 in.
Cutting Speed 20-24 in./min
Metal Thickness 1/2 in.
Tip Size 0 in.