Journeyman II EDGE 2.0

The robust Journeyman II EDGE 2.0 Outfit comes with everything you need to get started: CA 2460+ cutting attachment, WH 315FC+ welding handle, cutting tip, tip cleaner, striker, goggles, hose, welding nozzle and two EDGE 2.0 regulators. This heavy duty outfit cuts up to 8” (203.2 mm) and welds up to 3” (76.2 mm) with accessories.
Features
- ESS42 Series regulators
- WH 315FC+ torch handle with built-in fl ash arrestors and check valves
- CA2460+ cutting attachment
Industries
- Industrial and General Fabrication
- Repair and Maintenance
- Structural Steel Fabrication
- Light Fabrication