Eliminator - 16 Series Contact Tips

Eliminator - 16 Series Contact Tips

Tweco Eliminator 16 Series Contact Tips are made to last and do not utilize threads to secure the contact tip to the gas diffuser.

Add to shopping list


Features

  • Machined from a copper alloy tubing providing a consistent and smooth inside diameter surface
  • Patented contact tip providing a cam style connection into the mating gas diffuser
  • Used in standard duty welding application up to 200 amperes


Specifications