Previous Next

Tweco

15 Series Contact Tips

15 Series Contact Tips

Desinged for heavy duty welding environments, Tweco 15 Series Contact Tips are available from .035" - 1/16" standard; or .045 -1/8 heavy duty.

Where To Buy


Features

  • Easy identification - Each contact tip is marked showing Part No. and wire diameter
  • Excellent electrical properties
  • Inside diameter tolerance is held to +/-.003"
  • Machined from a copper alloy tubing providing a consistent and smooth inside diameter surface
  • Contact tips manufactured from extruded or gun-drilled copper alloy
  • Contact tips in either threaded and/or twist lock Eliminator style contact tips for
  • Eliminator style gas diffuser
  • Threaded style contact tip to ensure proper contact with a gas diffuser when installed to the MIG gun
  • Used in heavy-duty welding application up to 200 amperes
  • Slip-On or Thread-On nozzle styles with a choice of diameter bore sizes
  • Gas diffusers designed for specific MIG gun series
  • Contact tips in either threaded and/or twist lock Eliminator style contact tips for Eliminator style gas diffuser