ES 95i

ES 95i

The 95i DC Stick and Stick/TIG welding systems are lightweight at only 4.4 kg (9.7 lbs) for portability, suitable for outdoor use, and comes complete with everything you need to start welding.

Where To Buy


Features

  • DC output for TIG welding stainless, mild steel, and chrome molys
  • Lift TIG Start provides optimized TIG arc starting without the use of high frequency
  • 90 A of output capable of welding 2.4 mm (3/32 in.) electrodes
  • Fixed Hot Start & Arc Force for optimum Stick electrode performance
  • Overload Protection shuts down the power source to protect the internal electrical components


Industries

  • Hobbyist
  • Light Fabrication
  • Repair and Maintenance

Specifications

Dimensions

Height 9 in. (230 mm)
Length 13 in. (330 mm)
Width 5.1 in. (130 mm)

Input Voltage

Frequency 50/60 Hz
Phase 1
Voltage 104-127 V

Power Specifications

Protection Class IP23S

Specifications

Standards IEC 60974-1, CSA E60974-1, UL 60974-1