Stoody

Stoody 145-O

Stoody 145-O

Stoody 145 offers high abrasion resistance, high corrosion resistance and high hardness at elevated temperatures thanks to Niobium content - contributes to excellent high temperature abrasion resistance up to 1500°F (816°C).

Where To Buy


Features

  • High abrasion and corrosion resistance
  • Maintains hardness at elevated temperatures - up to 1500°F (816°C)
  • Can be applied to carbon, low alloy, and manganese steels


Specifications


Typical Tensile Properties

Hardness (HRC)
59-61 HRC

Typical Weld Metal Analysis %

OtherMoCCrFe
10.0 %6.0 %6.0 %24.0 %BAL %