Stoody 143-O

Stoody 143-O

Stoody 143 deposits consist of primary chromium carbides and secondary Niobium carbides in an austenitic matrix exhibiting high abrasion resistance and hardness up to 1100°F

Where To Buy


Features

  • High abrasion resistance
  • Maintains hardness up to 1100°F
  • Can be applied to carbon, low alloy, and manganese steels