Stoody PC2009-O

Stoody PC2009-O

Stoody PC2009 is a chromium carbide wire designed specifically for the application of abrasion resistant deposits inside pipe. The alloy is optimized to result in superior weldability for overlaying pipe ID in the flat position and elbows in the horizontal position. Stoody PC2009 can be used in hot wear applications up to 900°F (482°C).

Add to shopping list


Features

  • Designed specifically for pipe and elbow ID cladding
  • The alloy can be used in hot wear applications up to 900°F (482°C)


Specifications


Typical Tensile Properties

Hardness (HRC)
57-60 HRC

Typical Weld Metal Analysis %

OtherCCrFe
2.5 %5.5 %27 %BAL %