Stoody Foundry Co-Mang-O

Foundry Co-Mang is an austenitic manganese steel deposit which is suitable for multi-layer build-up and has excellent work hardening characteristics. It can also be used to join austenitic manganese steels.

Where To Buy


Specifications


Typical Tensile Properties

Hardness (BHN)
170-450 BHN

Typical Weld Metal Analysis %

OtherMnCFe
1.0 %16.0 %1.0 %BAL %