Stoody

Stoody 160

Typical Tensile Properties

75% Ar - 25% CO2
Hardness (HRC)
50-60 HRC

Typical Weld Metal Analysis %

OtherCWNiFe
2.0 %3.0 %41.0 %BAL %0.5 %

Deposition Data

75% Ar - 25% CO2
Diameter Current Deposition Type TTW Dist. Voltage Wire Feed Speed
1/16 in.
1.6 mm
150-200 A Full Range 1/2-5/8 in.
13-16 mm
18-20 V 90-110 in./min
229-279 cm/min