Stoody

Stoody 130

Typical Weld Metal Analysis %

OtherCWFe
0.5 %2.5 %58.0 %BAL %

Deposition Data

Full Range
Diameter Current TTW Dist. Voltage
1/16 in.
1.6 mm
150-200 A 1/2 in.
13 mm
17-19 V
7/64 in.
2.8 mm
300-350 A 1 in.
25 mm
18-22 V