Stoody

Stoody AC-DC Tube Borium

Typical Weld Metal Analysis %

ELEMENTVALUES
OtherCWFe
1.5 %2.5 %BAL %39.0 %

Deposition Data

Full Range
Diameter Current
3/16 in.
4.8 mm
120-150 A
1/4 in.
6.4 mm
140-165 A
1/8 in.
3.2 mm
80-100 A
5/32 in.
4.0 mm
100-120 A