Stoody 410NiMo

Stoody 410NiMo

Stoody AP stainless steel wires are designed for welding in all positions with Argon/CO2 gas mixtures or 100% CO2. These wires exhibit a spray like arc transfer, easy slag removal and can be welded within a wide range of parameters. Stoody 410NiMo T-1 AP wires can be used to join martensitic stainless steels such as type 410 used in valve and pump manufacturing. These wires can also be used for the repair and joining of ACICA6NM castings. AWS Classification: A5.22 E410NiMoT1-1/-4.

Add to shopping list


Specifications


Typical Weld Metal Analysis %

MnMoCSiNiCrFe
0.5 %0.6 %0.04 %0.4 %4.5 %12.0 %BAL %