All-State SEALCOR

All-State SEALCOR

A special aluminum flux cored brazing alloy for fabrication and repair of all weldable grades of aluminum including cast, sheet, and wrought. Ideal for out-of-position work, building up and joining dissimilar gauges of aluminum.

Where To Buy


Specifications


Typical Tensile Properties

Condition Tensile Strength Working Temperature
As Welded up to 30 ksi 1100 °F