All-State 31 Flux Cored

All-State 31 Flux Cored

Non-corrosive, non-hygroscopic flux inside a tubular rod; no separate flux required. For joining light gauge aluminum as used in furniture, truck and trailer bodies, window frames, aircraft instruments. Excellent color match but will darken if anodized. Very fluid, capillary action similar to silver brazing alloys.

Where To Buy


Specifications


Typical Tensile Properties

Condition Tensile Strength Working Temperature
As Welded up to 30 ksi 1075 °F