ESAB

OXWELD 1431 High Speed Series tips

Fuel Specifications

66Z60

Gas Pressure - Cutting Oxygen 80-115 psig
Gas Pressure - Preheat Oxygen 10 psig
Gas Pressure - Propane/NatGas 13 psig
Total Oxygen Consumption 1,850 cfh
Total Propane/NaturalGas Consumption 130 cfh

66Z61

Gas Pressure - Cutting Oxygen 80-115 psig
Gas Pressure - Preheat Oxygen 11 psig
Gas Pressure - Propane/NatGas 14 psig
Total Oxygen Consumption 2,100 cfh
Total Propane/NaturalGas Consumption 135 cfh

66Z62

Gas Pressure - Cutting Oxygen 80-115 psig
Gas Pressure - Preheat Oxygen 15 psig
Gas Pressure - Propane/NatGas 20 psig
Total Oxygen Consumption 3,100 cfh
Total Propane/NaturalGas Consumption 175 cfh

66Z63

Gas Pressure - Cutting Oxygen 80-115 psig
Gas Pressure - Preheat Oxygen 22 psig
Gas Pressure - Propane/NatGas 30 psig
Total Oxygen Consumption 4,700 cfh
Total Propane/NaturalGas Consumption 225 cfh

66Z64

Gas Pressure - Cutting Oxygen 60-80 psig
Gas Pressure - Preheat Oxygen 30 psig
Gas Pressure - Propane/NatGas 42 psig
Total Oxygen Consumption 4,900 cfh
Total Propane/NaturalGas Consumption 275 cfh

Operating Specifications

66Z60

Metal Thickness 6-10 in.
Tip Size 140 in.

66Z61

Metal Thickness 10-16 in.
Tip Size 160 in.

66Z62

Metal Thickness 16-20 in.
Tip Size 200 in.

66Z63

Metal Thickness 20-24 in.
Tip Size 240 in.

66Z64

Metal Thickness 24-28 in.
Tip Size 280 in.

Tip Specifications

Cleaning Drill Size Cutting 28
Cleaning Drill Size Preheat 54
Metal Thickness 6-10 in.
Tip Size 140 in.
Cleaning Drill Size Cutting 20
Cleaning Drill Size Preheat 53
Metal Thickness 10-16 in.
Tip Size 160 in.
Cleaning Drill Size Cutting 8
Cleaning Drill Size Preheat 52
Metal Thickness 16-20 in.
Tip Size 200 in.
Cleaning Drill Size Cutting C
Cleaning Drill Size Preheat 51
Metal Thickness 20-24 in.
Tip Size 240 in.
Cleaning Drill Size Cutting K
Cleaning Drill Size Preheat 50
Metal Thickness 24-28 in.
Tip Size 280 in.