ESAB

Rebel™ EMS 215ic

Rebel™ EMS 215ic

The Rebel™ EMS 215ic offers 120/230 V flexibility and some of the most innovative welding technology available. A breakthrough design inspired by professional welders, the Rebel EMS 215ic is a complete MIG/Stick welding package for mild steel, aluminum and stainless steel that goes where you go.

Where To Buy


Features

  • Excellent performance for best-in-class MIG, Flux-Cored and Stick welding, including 6010 Stick electrodes
  • Exclusive sMIG ("smart MIG") feature continuously learns and adapts to the operator’s welding technique to provide a stable arc and superior, repeatable welds; increases productivity for the experienced welder, and reduces training time for novice welders
  • Innovative display has larger display screen and higher pixel density to provide a more clear view of the TFT screen than other light industrial welders; loaded with exclusive features: on-demand availability of the user’s manual, listing of spare parts – all in multiple languages
  • Unique, five-handle roll cage industrial design and unibody steel construction in a lightweight, highly portable unit; 3-year handle-to-handle warranty
  • Rebel Series models come ready to weld out of the box with Professional Grade TWECO accessories and Victor gas regulator; shielding gas not included


Industries

  • Agricultural Equipment
  • Automotive
  • Automotive Bodies
  • Civil Construction
  • HVAC
  • Light Fabrication
  • Repair and Maintenance

Specifications

Arc Gun Consumables

Max Plate Thickness

Use With Welding Material 9.5 mm (3/8 in.)

Arc Holders Clamps & Misc

Cable 2m (6.5ft)

Power Specifications

Max Output (A) 240 A
Open Circuit Voltage 90 VDC
Protection Class IP23S
Supply Plug 230 V, NEMA 6-50P
Voltage Range (V) 10-26 V
Voltage Tolerance 95-270 V

Specifications

Standards CSA E60974-1-00, IEC 60974-1