This site uses cookies and other tracking technologies to provide you with our services, enhance the performance and functionality of our services, analyze the use of our products and services, and assist with our advertising and marketing efforts.

Cookie Policy   Privacy Notice

Previous Next

ESAB

Rebel™ EMP 215ic

Arc Gun Consumables

Max Plate Thickness

Use With Welding Material 9.5 mm (3/8 in.)

Arc Holders Clamps & Misc

Cable 2m (6.5ft)

Dimensions

Height 16 in. (406 mm)
Length 23 in. (584 mm)
Width 9 in. (229 mm)

Input Voltage

Frequency 50/60 Hz
Phase 1
Voltage 120; 208/230 V

Power Specifications

MIG Welding

Voltage Range (V) 10-26 V
Current Range(A) 5 – 150 A (120 V), 5 – 240 A (230 V) A
Max Output (A) 240 A
Open Circuit Voltage 68 VDC
Protection Class IP23S
Supply Plug 230 V, NEMA 6-50P
Voltage Range (V) 90-270 V
Voltage Steps Maximum 20
Voltage Steps Minimum 10

Specifications

Standards CSA E60974-1-00, IEC 60974-1

Weight

Weight 18.2 kg (40 lb)

Welding Output

Model Duty Cycle Output Current Output Voltage Welding Process
120 V 40 % 90 A 23.6 V Stick (SMAW)
120 V 40 % 130 A 15.2 V TIG (GTAW)
120 V 20 % 130 A 20.5 V MIG (GMAW)
230 V 25 % 180 A 27.2 V Stick (SMAW)
230 V 30 % 180 A 17.2 V TIG (GTAW)
230 V 25 % 205 A 24.3 V MIG (GMAW)

Wire Feeder Specifications

Max Spool Diameter 4, 8, 12 in. (100, 200, 300 mm)
Wire Feed Speed 1.5-12.1 m/min (59-476 in./min)
Metal Mild Steel
Wire Diameter .023-.035 in. (0.6-0.9 mm)
Metal Stainless Steel
Wire Diameter .030-.035 in. (0.8-0.9 mm)
Metal Aluminum
Wire Diameter .030-.045 in. (0.8-1.2 mm)
Metal Flux Cored
Wire Diameter .030-.045 in. (0.8-1.2 mm)