DUAL SHIELD 88-C3

DUAL SHIELD 88-C3

Dual Shield 88-C3 is a 1% nickel flux cored wire developed for low temperature impact toughness. It is an excellent choice for welding weathering grade steel, such as Cor-Ten® where W grade electrodes are not desireable. Dual Shield 88-C3 wire is recommended for welding high strength steels in the 70-80 ksi (483-552 MPa) tensile range. The weld metal analysis is similar to an E8018-C3 low hydrogen electrode.

Where To Buy


Industries

  • Barges
  • Bridge Construction
  • Civil Construction
  • General Cast Iron Repair and Fabrication
  • Power Generation
  • Railcars
  • Ship/Barge Building

Welding Process

  • Welding-FCAW - Flux Core Arc Welding

Specifications


Typical Tensile Properties

100% CO2
Condition Elongation Reduction in Area Tensile Strength Yield Strength
As Welded 28 % 60 % 86 ksi 75 ksi

Typical Charpy V-Notch Properties

100% CO2
Condition Impact Value Testing Temperature
As Welded 36 ft-lb -20 °F

Typical Weld Metal Analysis %

PMnCSSiNi
0.009 %1.0 %0.087 %0.015 %0.29 %0.95 %

Approvals: MIL; E-24403/1; MIL; 80T1-Ni1C
Classifications: ASME SFA 5.29; ASME SFA 5.36; AWS A5.36; E80T1-C1A2-Ni1; AWS A5.29; E80T1-Ni1C