FFRS Flux Feed and Recovery Systems

FFRS Flux Feed and Recovery Systems

Efficient flux handling for cost-effective welding

Where To Buy


Features

  • Ideal for continuous and high capacity welding
  • Minimum manual flux handling
  • Reduced flux consumption for better welding economy
  • Fewer weld stops for increased efficiency
  • Efficient filtration of used air
  • Flux feeds from a 20 gal. capacity TPC-75 pressurized flux tank to the ESAB flux hopper of your choice; 1.6 gal. or 2.6 gal.
  • Flux feed inlet options; straight or bent
FFRS Super
  • Built on OPC Super modules
  • Super stands for increased flux and heat conditions
  • Based on ejector vacuum principle
FFRS 2000 & 3000
  • Based on an electrical suction unit creating vacuum
  • For use when extra high recovery force is required and for compact welding heads
  • Flux dust separated automatically in a pre-separator