This site uses cookies and other tracking technologies to provide you with our services, enhance the performance and functionality of our services, analyze the use of our products and services, and assist with our advertising and marketing efforts.

Cookie Policy   Privacy Notice

Previous Next

ESAB

A2S Mini Master

Capacities

Flux Hopper Capacity (Single Wire SAW) 1.4 gal (6 l)
Flux Hopper Capacity (Twin Wire SAW) 1.4 gal (6 l)
Linerar Slide Stroke Length 3.5 in. (90 mm)
Rotary Slide Setting Range (deg) 360 °

Power Requirements

Control Voltage 42 VAC

Wire/Strip Specifications

Model Wire Diameter, Single Wire Feed Speed Wire Type
GMAW .030-1/16 in.
0.8-1.6 mm
630 in./min
16 m/min
Steel
GMAW .030-1/16 in.
0.8-1.6 mm
630 in./min
16 m/min
Stainless Steel
GMAW .045-3/32 in.
1.2-2.4 mm
630 in./min
16 m/min
Cored Wire
GMAW .045-1/16 in.
1.2-1.6 mm
630 in./min
16 m/min
Aluminium
GMAW MTW 600w .040-1/16 in.
1.0-1.6 mm
984 in./min
25 m/min
Steel
GMAW MTW 600w .040-1/16 in.
1.0-1.6 mm
984 in./min
25 m/min
Stainless Steel
GMAW MTW 600w .040-3/32 in.
1.0-2.4 mm
984 in./min
25 m/min
Cored Wire
GMAW MTW 600w .040-5/64 in.
1.0-2.0 mm
984 in./min
25 m/min
Aluminium
Single Wire SAW 1/16-5/32 in.
1.6-4.0 mm
354 in./min
9 m/min
Steel
Single Wire SAW 1/16-5/32 in.
1.6-4.0 mm
354 in./min
9 m/min
Stainless Steel
Single Wire SAW 1/16-5/32 in.
1.6-4.0 mm
354 in./min
9 m/min
Cored Wire
Twin Wire SAW 2x.045-3/32 in.
2x1.2-2.5 mm
354 in./min
9 m/min
Steel