OK Tigrod 5356 is the most widely used welding alloy and can be classified as a general purpose type filler alloy. OK Tigrod 5356 is typically chosen because of its relatively high shear strength. The 5XXX alloy base material, welded with OK Tigrod 5356, with a weld pool chemistry greater than 3 % Mg and service temperatures in excess of 65°C are susceptible to stress corrosion cracking. The alloy is non-heat treatable.

Add to shopping list


Specifications


Typical Tensile Properties

Condition Elongation Tensile Strength Yield Strength
As Welded 17 % 34 ksi 16 ksi

Typical Weld Metal Analysis %

MnCuZnSiMgAlCrFe
0.13 %0.01 %0.01 %0.05 %4.9 %94.560 %0.12 %0.13 %

Approvals: ABS, R 5356, CE, EN 13479, CWB, A5.10/A5.10M:2012 ER5356, DB, 61.039.02, JIS, JIS Z 3232, VdTÜV, 04665
Classifications: JIS Z 3232, A5356, SFA/AWS A5.10, R5356, Wire Electrode, EN ISO 18273, S Al 5356 (AlMg5Cr(A)), Wire Electrode

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Type: AlMg 5