Previous Next

ESAB

OK Tigrod 4043

OK Tigrod 4043

OK Tigrod 4043 is one of the most widely used welding alloys. The alloy is used for welding AlMgSi - types and AlSi - alloys with up to 7% Silicon. Not recommended for anodizing. Non-heat treatable.

Add to shopping list


Specifications


Typical Tensile Properties

As welded
Elongation Tensile Strength Yield Strength
18 % 18 ksi 8 ksi

Typical Weld Metal Analysis %

MnCuZnTiSiAlFe
0.01 %0.02 %0.01 %0.01 %5.00 %Rem %0.14 %

Approvals: CE, EN 13479, DB, 61.039.06, JIS, JIS Z 3232, For lot numbers starting with RB, CWB, AWS A5.10/A5.10M:2012 (ER4043), For lot numbers starting with RB
Classifications: SFA/AWS A5.10, R4043, Wire Electrode, EN ISO 18273, S Al 4043 (AlSi5), Wire Electrode, JIS Z 3232, A4043, Wire Electrode

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Type: AlSi