CaB System 300S/300M

CaB System 300S/300M

Flexible, Modular Column and Booms


Features

ESAB offers a totally integrated solution including welding process, manipulator movement as well as control of third axis products like the ESAB roller beds or positioners

  • Modular design concept allows total customization using standard components
  • Large selection of available components to integrate for a custom solution:
  • A variety of welding heads for SAW but also GMAW and GTAW
  • A complete range of rectifiers, transformers and inverter based power sources
  • The welding process is controlled from ESAB PEK or a PLC system
  • ESAB flux feeding and recovery systems
  • Monitoring systems and cameras
  • Choose from stationary or mobile, rail-travelling carriage systems
  • A Column and Boom ranging from 3x3 to 5x5 meter working range as standard
  • Single or twin wire set-up with the A2 or A6 welding head
  • 30 kg wire spools


Specifications

Weights

Concrete Stand Total Weight 1550 kg (3417 lb)
Foot Plate Total Weight 350 kg (772 lb)
Rail Carriage Total Weight 1670 kg (3681 lb)