A6 Mastertrac A6TF (Single/Twin SAW)

Capacities and Temperatures

Model Single SAW Single/Twin SAW Single/Twin SAW (high speed) Twin SAW
Flux Capacity 2.6 gal
10 l
Wire Diameter 1/8-1/4 in.
3.0-6.0 mm
2x3/32-1/8 in.
Wire Feed Speed 8-157.5 in./min
0.2-4.0 m/min
16-315 in./min
0.4-8 m/min
Wire Spool Capacity 66 lb
30 kg
2x66 lb
2x30 kg
Wire Type 2x2.0-3.0

Measurements and Dimensions

Model Weight
Single SAW 242.5 lb
110 kg
Twin SAW 242.5 lb
110 kg

Power Requirements

Model Single/Twin SAW
Conditional Qualification @ 100% Duty Cycle
Connection Voltage 42 VAC
Permissible Load 1500 A

Specifications

Wire Diameter 0.045-1/8 in. (1.0-3.2 mm)
Wire Diameter 3/32-1/8 in. (2.0-3.0 mm)
Wire Diameter 1/8-1/4 in. (3.0-6.0 mm)

Weight

Twin SAW

Weight 110 kg (242.5 lb)

Single SAW

Weight 110 kg (242.5 lb)

Welding Speeds

Travel Speed 0.1-2.0 m/min (4-79 in./min)