A2 Tripletrac A2TF

Capacities and Temperatures

Wire Spool Capacity 30 kg (66 lb)
Flux Capacity 1.4 gal (6 l)
Wire Feed Speed 354 in./min (9 m/min)
Wire Diameter 1/16-5/32 in. (1.6-4.0 mm)
Wire Type Steel
Wire Diameter 1/16-5/32 in. (1.6-4.0 mm)
Wire Type Stainless Steel
Wire Diameter 1/16-5/32 in. (1.6-4.0 mm)
Wire Type Cored Wire

Measurements and Dimensions

Linear Slides Setting Length 3.5 in. (90 mm)
Max Inclination 5 °
Weight 103 lb (47 kg)

Power Requirements

Permissible Load (@ 100% duty cycle) 800 A
Connection Voltage 42 VAC

Specifications

Wire Diameter 1/16-5/32 in. (1.6-4.0 mm)

Welding Speeds

Travel Speed 0.1-1.7 m/min (4-67 in./min)