Previous Next

ESAB

A2 Multitrac with A2-A6 Process Controller PEK

Capacities and Temperatures

Model Flux Capacity Wire Feed Speed Wire Spool Capacity
GMAW 16 m/min 60 lb
30 kg
MTW600 (GMAW) 25 m/min 2x33 lb
2x15 kg
Single SAW 1.4 gal
6 l
354 in./min
9 m/min
60 lb
30 kg
Twin SAW 1.4 gal
6 l
354 in./min
9 m/min
2x33 lb
2x15 kg

Power Requirements

Model Max Current
GMAW 600 A
SAW 800 A

Specifications

Model Metal Type Wire Diameter
GMAW Steel 0.8-1.6 mm
GMAW Stainless Steel 0.8-1.6 mm
GMAW Cored Wire 1.2-2.4 mm
GMAW Aluminum 1.2-1.6 mm
MTW600 (GMAW) Steel 0.8-1.6 mm
MTW600 (GMAW) Stainless Steel 0.8-1.6 mm
MTW600 (GMAW) Cored Wire 1.2-1.6 mm
MTW600 (GMAW) Aluminum 1.2-2.0 mm
Single SAW Steel 1.6-4.0 mm
Single SAW Stainless Steel 1.6-4.0 mm
Single SAW Cored Wire 1.6-4.0 mm
Single SAW Aluminum
Twin SAW Steel 2x1.2-2.5 mm
Twin SAW Stainless Steel 2x1.2-2.5 mm
Twin SAW Cored Wire
Twin SAW Aluminum

Weights & Dimensions

Model GMAW SAW
Height 828 mm 828 mm
Length 527 mm 527 mm
Weight 43 kg 47 kg
Width 375 mm 375 mm

Welding Speeds

Travel Speed 0.1-2.0 m/min (4-79 in./min)
x
×

Find the Closest Distributor

x

Find the Closest Distributor

x

x

Loading..