ESAB

TIGROD ER80S-B8

TIGROD ER80S-B8

ER80S-B8 is a non-copper-coated solid wire for TIG welding requiring creep strength. This 9% Chromium - 1% Molybdenum TIG rod is used to weld 9% Chromium - 1% Molybdenum steels (ASTM Section IX, P No 5B, Group 1) such as ASTM A335 Grade P9 or ASTM A213 Grade T9. Tigrod products are embossed on opposite ends with the alloy identification.

Where To Buy


Industries

  • Power Generation

Welding Process

  • Welding-GTAW (TIG - Tungsten Inert Gas )

Specifications


Typical Tensile Properties

Condition Elongation Stress Relieved Temperature Stress Relieved Testing Time Tensile Strength Yield Strength
Stress Relieved 24 % 1375 °F 1 hr 97 ksi 78 ksi

Typical Weld Metal Analysis %

ELEMENTVALUES
PMnX-FactorCuMoSCSiNiCr
0.005 %0.50 %< 15 %max 0.20 %1.00 %0.003 %0.07 %0.40 %max 0.50 %9.00 %

Classifications: ASME SFA 5.28; AWS A5.28; ER80S-B8