SUREWELD 7024

Typical Tensile Properties

Condition Elongation Reduction in Area Tensile Strength Yield Strength
As Welded 26 % 63 % 81 ksi 71 ksi

Typical Charpy V-Notch Properties

Condition Impact Value Testing Temperature
As Welded 25 ft-lb 0 °F

Typical Weld Metal Analysis %

PMnCSSi
0.01 %0.80 %0.06 %0.018 %0.30 %

Deposition Data

Diameter Current Deposition Rate Efficiency (%) Optimal Amps
3/16 in.
4.8 mm
250-290 A 7.5 lb/h
3.4 kg/h
69.2 % 245 A
3/16 in.
4.8 mm
250-290 A 8.3 lb/h
3.8 kg/h
70.5 % 270 A
3/16 in.
4.8 mm
250-290 A 9.1 lb/h
4.1 kg/h
68 % 290 A
7/32 in.
5.6 mm
300-340 A 9.4 lb/h
4.3 kg/h
72.4 % 320 A
7/32 in.
5.6 mm
300-340 A 11.6 lb/h
5.3 kg/h
69.1 % 360 A
1/4 in.
6.4 mm
350-400 A 12.6 lb/h
5.7 kg/h
71.7 % 400 A
5/32 in.
4.0 mm
180-240 A 5.3 lb/h
2.4 kg/h
71.3 % 180 A
5/32 in.
4.0 mm
180-240 A 6.3 lb/h
2.9 kg/h
72.5 % 210 A
5/32 in.
4.0 mm
180-240 A 7.2 lb/h
3.3 kg/h
69.4 % 240 A

Approvals: CWB CSA W48, E4924
Classifications: ASME SFA 5.1, AWS A5.1, E7024