SUREWELD 7024

SUREWELD 7024

Sureweld 7024 is a high speed, heavy-coated, iron powder electrode for high deposition rates on horizontal and downhand welding. Excellent operator appeal, produces equal 45° fillets, thereby eliminating over welding. Excellent bead appearance and self-cleaning slag. This electrode has good weldability and superior mechanical properties. It is particularly useful in obtaining increased penetration with little or no root porosity in horizontal or positioned fillets. Sureweld 7024 is ideal for making high speed horizontal fillet and lap welds on mild and some alloy steels, such as earthmoving and construction equipment, truck bodies, ships, barges and railcars. Sureweld 7024 exceeds the AWS A5.1 elongation % and Charpy V-Notch requirements for 7024-1.

Where To Buy


Industries

  • Barges
  • Industrial and General Fabrication
  • Mobile Equipment
  • Railcars

Welding Process

  • Welding-SMAW/MMA (Stick)

Specifications


Typical Tensile Properties

Condition Elongation Reduction in Area Tensile Strength Yield Strength
As Welded 26 % 63 % 81 ksi 71 ksi

Typical Charpy V-Notch Properties

Condition Impact Value Testing Temperature
As Welded 25 ft-lb 0 °F

Typical Weld Metal Analysis %

PMnCSSi
0.01 %0.80 %0.06 %0.018 %0.30 %

Approvals: CWB CSA W48, E4924
Classifications: ASME SFA 5.1, AWS A5.1, E7024