TIGROD ER80S-B6

TIGROD ER80S-B6

Tigrod ER80S-B6 is a Chrome-Moly TIG rod for joining 5% Cr - 0.5% Mo steels such as ASTM A200-T5, A335-P5 and A387-Gr5. These non-copper-coated rods are primarily used to fabricate and repair power piping, pressure vessels, heat exchangers, and boilers used in the power generation industry. All ESAB ER80S-B6 Tigrod is embossed on both ends with the alloy identification. This grade of rod was previously classified as ER502.

Where To Buy


Industries

  • Petrochemical
  • Process

Welding Process

  • Welding-GTAW (TIG - Tungsten Inert Gas )

Specifications


Typical Tensile Properties

Condition Elongation Stress Relieved Temperature Stress Relieved Testing Time Tensile Strength Yield Strength
Stress Relieved 24 % 1350 °F 1 hr 95 ksi 82 ksi
Stress Relieved 26 % 1375 °F 1 hr 93 ksi 80 ksi

Typical Weld Metal Analysis %

PMnX-FactorCuMoSCVSiNiCr
0.007 %0.50 %< 15 %max 0.20 %0.50 %0.01 %0.08 %max 0.03 %0.40 %max 0.3 %5.80 %

Classifications: ASME SFA 5.28, AWS A5.28, ER80S-B6