TIGROD ER80S-B2

TIGROD ER80S-B2

Tigrod ER80S-B2 is a chrome-moly TIG rod used for joining creep resistant steels of the 0.5% Cr - 0.5% Mo, 1% Cr - 0.5% Mo, and 1.25% Cr - 0.5% Mo grades. These non-copper-coated rods are primarily used to fabricate and repair power piping and boilers in the power generation industry.

Where To Buy


Industries

  • Process
  • Petrochemical

Welding Process

  • Welding-GTAW (TIG - Tungsten Inert Gas )

Specifications


Typical Tensile Properties

Condition Elongation Stress Relieved Temperature Stress Relieved Testing Time Tensile Strength Yield Strength
Stress Relieved 29 % 1150 °F 1 hr 95 ksi 81 ksi
Stress Relieved 24 % 1350 °F 1 hr 95 ksi 82 ksi
Stress Relieved 26 % 1375 °F 1 hr 93 ksi 80 ksi

Typical Weld Metal Analysis %

ELEMENTVALUES
PMnX-FactorCuMoSCVSiNiCr
max 0.012 %0.40-0.70 %max 12 %max 0.20 %0.40-0.65 %max 0.025 %0.07-0.012 %max 0.03 %0.40-0.70 %max 0.20 %1.20-1.50 %

Classifications: AWS A5.28; ER80S-B2