ESAB

Origo Mig 320/410

Dimensions

Origo Mig 320

Height 32 in.
Length 33 in.
Width 16 in.

Origo Mig 410

Height 36 in.
Length 32 in.
Width 21 in.

Input Voltage

Model Origo Mig 320 Origo Mig 410
Frequency 50/60 Hz 60 Hz
Phase 3 3
Voltage 230/460 V 230/460 V

Power Specifications

Model Origo Mig 320 Origo Mig 410
Current Range(A) 40-320 A 50-400 A
Efficiency at Maximum Current 75 % 71 %
Open Circuit Power W 200 W 360 W
Open Circuit Voltage 16-40 VAC 17-45 VAC
Power Factor at Maximum Current 0.94 0.98
Protection Class IP 23 IP 23
Voltage Range (V) 16-30 V 16.5-34 V
Voltage Steps Minimum 40 40

Specifications

Operating Temp -10 to 40 °C (14 to 104 °F)

Weight

Origo Mig 320

Weight 244 lb

Origo Mig 410

Weight 317 lb

Origo Mig 410 w/cooling unit

Weight 348 lb

Welding Output

Model Duty Cycle Output Current Output Voltage
Origo Mig 320 30 % 320 A 30 VAC
Origo Mig 320 60 % 250 A 27 VAC
Origo Mig 320 100 % 195 A 24 VAC
Origo Mig 410 50 % 400 A 34 VAC
Origo Mig 410 60 % 365 A 32 VAC
Origo Mig 410 100 % 280 A 28 VAC