This site uses cookies and other tracking technologies to provide you with our services, enhance the performance and functionality of our services, analyze the use of our products and services, and assist with our advertising and marketing efforts.

Cookie Policy   Privacy Notice

Previous Next

ESAB

MIGMASTER 215 Pro/280 Pro

Dimensions

Migmaster 215 Pro

Height 32.7 in.
Length 33 in.
Width 16.7 in.

Migmaster 280 Pro

Height 36.5 in.
Length 32 in.
Width 22 in.

Input Voltage

Model 215 Pro / 280 Pro 280 Pro
Frequency 60 Hz 60 Hz
Phase 1 1
Voltage 208/230 V 230/460/575 V

Power Specifications

Model 215 Pro 280 Pro
Creep Start Selectable Selectable
Current Range(A) 40-250 A 40-300 A
Efficiency at Maximum Current 76 % 71 %
Power Factor at Maximum Current 0.95 0.97
Protection Class IP23S IP23S
Voltage Range (V) 16-23 V 16-29 V
Voltage Steps Minimum 12 21

Specifications

Burnback Time 0-0.25 sec
Operating Temp -10 to 40 °C (14 to 104 °F)
Spot Weld Time 0.2-2.5 sec

Weight

Migmaster 215 Pro

Weight 216 lb

Migmaster 280 Pro

Weight 308 lb

Welding Output

Model Duty Cycle Output Current Output Voltage
215 Pro 20 % 250 A 23 V
215 Pro 40 % - A - V
215 Pro 60 % 160 A 22 V
215 Pro 100 % 110 A 19.5 V
280 Pro 20 % - A - V
280 Pro 40 % 300 A 29 V
280 Pro 60 % 250 A 26.5 V
280 Pro 100 % 194 A 23.7 V