Previous Next

ESAB

HW-25

HW-25

Water-Cooled Torch Family - 200 amp

Where To Buy


Features

  • Small, Lightweight
  • Flexible head to access difficult joints

Specifications

Specifications

Cooling Requirements 0.25 gal

Weight

less service lines

Weight 14 oz