SPOOLARC 95

Spoolarc 95 is Military grade high strength wire used to weld HY-80 steels. Applications for Spoolarc 95 include military tanks, ships and submarines.

Where To Buy


Industries

  • Heavy Fabrication
  • Military Applications
  • Mining
  • Ship/Barge Building

Welding Process

  • Welding-GMAW (MIG/MAG - Metal Inert Gas / Metal Active Gas)

Specifications


Typical Tensile Properties

Condition Elongation Tensile Strength Yield Strength
As Welded 23 % 105 ksi 95 ksi

Typical Charpy V-Notch Properties

75% Ar - 25% CO2
Condition Impact Value Testing Temperature
As Welded 65 ft-lb -60 °F
As Welded 93 ft-lb 0 °F

Typical Weld Metal Analysis %

PMnMoSCVSiNiCr
0.004 %1.35 %0.34 %0.008 %0.06 %0.001 %0.33 %1.75 %0.1 %

Approvals: CWB, CSA W48, MIL-E-100S-1/MIL-E-23765/2
Classifications: AWS A5.28, ER100S-1