Typical Tensile Properties

98% Ar - 2% O2
Condition Elongation Tensile Strength Yield Strength
As Welded 22 % 110 ksi 95 ksi
100% CO2
Condition Elongation Tensile Strength Yield Strength
As Welded 23 % 92 ksi 77 ksi

Typical Charpy V-Notch Properties

100% CO2
Condition Impact Value Testing Temperature
As Welded 44 ft-lb -20 °F
98% Ar - 2% O2
Condition Impact Value Testing Temperature
As Welded 87 ft-lb -20 °F

Typical Weld Metal Analysis %

ELEMENTVALUES
PMnCuMoCSSiNi
0.01 %1.69 %0.17 %0.4 %0.08 %0.011 %0.63 %0.09 %

Deposition Data

Spray Transfer
Diameter Current Deposition Rate Voltage Wire Feed Speed
1/16 in.
1.6 mm
370 A 13.2 lb/h
6.0 kg/h
34 V 260 in./min
660 cm/min
.035 in.
0.9 mm
197 A 7.1 lb/h
3.2 kg/h
26 V 450 in./min
1143 cm/min
1/16 in.
1.6 mm
390 A 14.2 lb/h
6.4 kg/h
36 V 280 in./min
771 cm/min
.035 in.
0.9 mm
213 A 7.9 lb/h
3.6 kg/h
26 V 500 in./min
1270 cm/min
.045 in.
1.2 mm
260 A 7.9 lb/h
3.6 kg/h
25 V 300 in./min
762 cm/min
.035 in.
0.9 mm
230 A 8.7 lb/h
4.0 kg/h
27 V 550 in./min
1397 cm/min
.045 in.
1.2 mm
280 A 9.2 lb/h
4.2 kg/h
26 V 350 in./min
889 cm/min
.045 in.
1.2 mm
300 A 10.5 lb/h
4.8 kg/h
28 V 400 in./min
1016 cm/min
.045 in.
1.2 mm
320 A 11.8 lb/h
5.4 kg/h
29 V 450 in./min
1143 cm/min
.045 in.
1.2 mm
340 A 13.1 lb/h
6.0 kg/h
30 V 500 in./min
1270 cm/min
.030 in.
0.8 mm
160 A 5.8 lb/h
2.6 kg/h
24 V 500 in./min
1270 cm/min
.052 in.
1.3 mm
275 A 9.3 lb/h
4.2 kg/h
26 V 265 in./min
673 cm/min
.052 in.
1.3 mm
310 A 10.5 lb/h
4.8 kg/h
28 V 300 in./min
762 cm/min
.052 in.
1.3 mm
360 A 12.2 lb/h
5.6 kg/h
31 V 350 in./min
889 cm/min
.052 in.
1.3 mm
400 A 12.2 lb/h
5.6 kg/h
33 V 390 in./min
991 cm/min
1/16 in.
1.6 mm
290 A 9.1 lb/h
4.1 kg/h
26 V 180 in./min
457 cm/min
1/16 in.
1.6 mm
310 A 10.1 lb/h
4.6 kg/h
28 V 200 in./min
508 cm/min
.030 in.
0.8 mm
173 A 6.4 lb/h
2.9 kg/h
25 V 550 in./min
1397 cm/min
.030 in.
0.8 mm
187 A 7.0 lb/h
3.2 kg/h
25 V 600 in./min
1524 cm/min
1/16 in.
1.6 mm
340 A 11.6 lb/h
5.3 kg/h
31 V 230 in./min
584 cm/min
.035 in.
0.9 mm
180 A 6.3 lb/h
2.9 kg/h
25 V 400 in./min
1016 cm/min
.030 in.
0.8 mm
200 A 7.6 lb/h
3.4 kg/h
26 V 650 in./min
1651 cm/min

Deposition Data

Short Arc Transfer
Diameter Current Deposition Rate Voltage Wire Feed Speed
.030 in.
0.8 mm
60 A 1.7 lb/h
0.8 kg/h
14 V 150 in./min
381 cm/min
.030 in.
0.8 mm
80 A 2.2 lb/h
1.0 kg/h
15 V 200 in./min
508 cm/min
.030 in.
0.8 mm
100 A 2.8 lb/h
1.3 kg/h
15 V 250 in./min
635 cm/min
.035 in.
0.9 mm
90 A 2.7 lb/h
1.2 kg/h
15 V 180 in./min
457 cm/min
.030 in.
0.8 mm
120 A 3.3 lb/h
1.5 kg/h
16 V 300 in./min
762 cm/min
.035 in.
0.9 mm
113 A 3.3 lb/h
1.5 kg/h
16 V 220 in./min
559 cm/min
.030 in.
0.8 mm
140 A 3.9 lb/h
1.7 kg/h
16 V 350 in./min
889 cm/min
.035 in.
0.9 mm
137 A 4.0 lb/h
1.8 kg/h
18 V 260 in./min
660 cm/min
.030 in.
0.8 mm
144 A 4.0 lb/h
1.8 kg/h
16 V 360 in./min
914 cm/min
.035 in.
0.9 mm
160 A 4.6 lb/h
2.1 kg/h
19 V 300 in./min
762 cm/min
.045 in.
1.2 mm
130 A 3.1 lb/h
1.4 kg/h
17 V 125 in./min
318 cm/min
.045 in.
1.2 mm
163 A 4.0 lb/h
1.8 kg/h
18 V 160 in./min
406 cm/min
.052 in.
1.3 mm
150 A 4.5 lb/h
2.1 kg/h
17 V 135 in./min
343 cm/min
.052 in.
1.3 mm
173 A 5.4 lb/h
2.4 kg/h
18 V 160 in./min
406 cm/min
.052 in.
1.3 mm
200 A 6.4 lb/h
2.9 kg/h
20 V 190 in./min
483 cm/min
.045 in.
1.2 mm
200 A 5.0 lb/h
2.3 kg/h
19 V 200 in./min
508 cm/min

Approvals: CWB; CAN/CSA-ISO14341,B-G 55A 3 G4M31 (ER80S-D2); CWB; CSA W48; MIL-E-23765/2; 80S-3
Classifications: AWS A5.28; ER80S-D2/ER90S-D2