SPOOLARC 83

SPOOLARC 83

Spoolarc 83 contains 0.5% Mo to provide higher deposit strength in both the as welded and stress relieved conditions. It contains high levels of Manganese and Silicon to provide good wetting and good rust and scale tolerance. Spoolarc 83 is also used for all-position welding of high tensile pipe and tubing commonly found in earthmoving and construction equipment. It is available in forms suitable for MIG and TIG welding.

Where To Buy


Industries

  • Automotive
  • Industrial and General Fabrication
  • Mobile Equipment
  • Ship/Barge Building

Welding Process

  • Welding-GMAW (MIG/MAG - Metal Inert Gas / Metal Active Gas)
  • Welding-GTAW (TIG - Tungsten Inert Gas )
  • Welding-SAW - Submerged Arc Welding

Specifications


Typical Tensile Properties

98% Ar - 2% O2
Condition Elongation Tensile Strength Yield Strength
As Welded 22 % 110 ksi 95 ksi
100% CO2
Condition Elongation Tensile Strength Yield Strength
As Welded 23 % 92 ksi 77 ksi

Typical Charpy V-Notch Properties

100% CO2
Condition Impact Value Testing Temperature
As Welded 44 ft-lb -20 °F
98% Ar - 2% O2
Condition Impact Value Testing Temperature
As Welded 87 ft-lb -20 °F

Typical Weld Metal Analysis %

PMnCuMoCSSiNi
0.01 %1.69 %0.17 %0.4 %0.08 %0.011 %0.63 %0.09 %

Approvals: CWB, CAN/CSA-ISO14341,B-G 55A 3 G4M31 (ER80S-D2), CWB, CSA W48, MIL-E-23765/2, 80S-3
Classifications: AWS A5.28, ER80S-D2/ER90S-D2

Approvals are based on factory location. Please contact ESAB for more information.