SPOOLARC 75

Typical Tensile Properties

98% Ar - 2% O2
Condition Elongation Tensile Strength Yield Strength
As Welded 31 % 81 ksi 70 ksi

Typical Charpy V-Notch Properties

98% Ar - 2% O2
Condition Impact Value Testing Temperature
As Welded 100 ft-lb -50 °F

Typical Weld Metal Analysis %

ELEMENTVALUES
PMnMoCuSCSiNiCr
0.01 %0.94 %0.01 %0.08 %0.002 %0.08 %0.49 %0.98 %0.04 %

Deposition Data

Diameter Current Deposition Rate Efficiency (%)
5/32 in.
4.0 mm
800 A 23.0 lb/h
10.4 kg/h
99 %
3/32 in.
2.4 mm
400 A 13.2 lb/h
6 kg/h
99 %
5/32 in.
4.0 mm
900 A 26.0 lb/h
11.8 kg/h
99 %
3/32 in.
2.4 mm
500 A 17.0 lb/h
7.7 kg/h
99 %
3/32 in.
2.4 mm
600 A 22.0 lb/h
10 kg/h
99 %
1/8 in.
3.2 mm
400 A 11.0 lb/h
5 kg/h
99 %
1/8 in.
3.2 mm
500 A 14.5 lb/h
6.6 kg/h
99 %
1/8 in.
3.2 mm
600 A 18.0 lb/h
8.2 kg/h
99 %
1/8 in.
3.2 mm
700 A 21.2 lb/h
9.6 kg/h
99 %
5/32 in.
4.0 mm
500 A 12.5 lb/h
5.7 kg/h
99 %
5/32 in.
4.0 mm
600 A 16.0 lb/h
7.3 kg/h
99 %
5/32 in.
4.0 mm
700 A 19.5 lb/h
8.8 kg/h
99 %

Classifications: ASME SFA 5.28; ASME SFA 5.23; AWS A5.28; ER80S-Ni1; AWS A5.23; ENi1K