Typical Tensile Properties

90% Ar - 10% CO2
Condition Elongation Tensile Strength Yield Strength
As Welded 29 % 86 ksi 73 ksi

Typical Charpy V-Notch Properties

90% Ar - 10% CO2
Condition Impact Value Testing Temperature
As Welded 96 ft-lb -50 °F
As Welded 91 ft-lb -40 °F
As Welded 115 ft-lb -20 °F

Typical Weld Metal Analysis %

ELEMENTVALUES
PMnMoCuSCSiNiCr
0.008 %1.51 %0.01 %0.11 %0.01 %0.08 %0.85 %0.01 %0.02 %

Deposition Data

Diameter Current Deposition Rate Efficiency (%)
.030 in.
0.8 mm
75 A 1.8 lb/h
0.82 kg/h
93 %
.030 in.
0.8 mm
100 A 2.5 lb/h
1.13 kg/h
93 %
.030 in.
0.8 mm
150 A 3.9 lb/h
1.77 kg/h
93 %
.030 in.
0.8 mm
200 A 6.5 lb/h
2.95 kg/h
93 %

Deposition Data

92% Ar - 8% CO2
Diameter Current Deposition Rate Efficiency (%)
1/16 in.
1.6 mm
350 A 11.3 lb/h
5.13 kg/h
98 %
.035 in.
0.9 mm
150 A 4.2 lb/h
1.90 kg/h
98 %
.045 in.
1.2 mm
125 A 2.8 lb/h
1.27 kg/h
98 %
.030 in.
0.8 mm
100 A 2.6 lb/h
1.18 kg/h
98 %
.045 in.
1.2 mm
300 A 10.2 lb/h
4.63 kg/h
98 %
1/16 in.
1.6 mm
400 A 14.0 lb/h
6.35 kg/h
98 %
.035 in.
0.9 mm
200 A 6.2 lb/h
2.81 kg/h
98 %
.045 in.
1.2 mm
150 A 3.6 lb/h
1.63 kg/h
98 %
.030 in.
0.8 mm
150 A 4.1 lb/h
1.86 kg/h
98 %
.045 in.
1.2 mm
350 A 13.2 lb/h
5.99 kg/h
98 %
1/16 in.
1.6 mm
450 A 17.4 lb/h
7.89 kg/h
98 %
.045 in.
1.2 mm
200 A 5.6 lb/h
2.54 kg/h
98 %
1/16 in.
1.6 mm
250 A 6.5 lb/h
2.95 kg/h
98 %
1/16 in.
1.6 mm
275 A 7.7 lb/h
3.49 kg/h
98 %
1/16 in.
1.6 mm
300 A 9.0 lb/h
4.08 kg/h
98 %
.035 in.
0.9 mm
250 A 9.0 lb/h
4.08 kg/h
98 %
.030 in.
0.8 mm
200 A 6.8 lb/h
3.08 kg/h
98 %
.035 in.
0.9 mm
100 A 2.7 lb/h
1.22 kg/h
98 %
.045 in.
1.2 mm
100 A 2.1 lb/h
0.95 kg/h
98 %
.035 in.
0.9 mm
80 A 2.2 lb/h
1.00 kg/h
98 %
.045 in.
1.2 mm
250 A 7.8 lb/h
3.58 kg/h
98 %
.030 in.
0.8 mm
75 A 2.0 lb/h
0.91 kg/h
98 %

Deposition Data

75% Ar - 25% CO2
Diameter Current Deposition Rate Efficiency (%)
.045 in.
1.2 mm
125 A 2.8 lb/h
1.27 kg/h
96 %
.030 in.
0.8 mm
100 A 2.6 lb/h
1.18 kg/h
96 %
.045 in.
1.2 mm
300 A 10.0 lb/h
4.53 kg/h
96 %
1/16 in.
1.6 mm
400 A 13.7 lb/h
6.21 kg/h
96 %
.035 in.
0.9 mm
200 A 6.0 lb/h
2.72 kg/h
96 %
.045 in.
1.2 mm
150 A 3.5 lb/h
1.59 kg/h
96 %
.030 in.
0.8 mm
150 A 4.0 lb/h
1.81 kg/h
96 %
.045 in.
1.2 mm
350 A 12.9 lb/h
5.85 kg/h
96 %
1/16 in.
1.6 mm
450 A 17.1 lb/h
7.76 kg/h
96 %
.035 in.
0.9 mm
250 A 8.8 lb/h
3.09 kg/h
96 %
.045 in.
1.2 mm
200 A 5.5 lb/h
2.49 kg/h
96 %
.045 in.
1.2 mm
100 A 2.0 lb/h
0.91 kg/h
96 %
1/16 in.
1.6 mm
250 A 6.4 lb/h
2.90 kg/h
96 %
1/16 in.
1.6 mm
275 A 7.6 lb/h
3.45 kg/h
96 %
1/16 in.
1.6 mm
300 A 8.8 lb/h
3.99 kg/h
96 %
.030 in.
0.8 mm
200 A 6.7 lb/h
3.04 kg/h
96 %
.035 in.
0.9 mm
100 A 2.7 lb/h
1.22 kg/h
96 %
.035 in.
0.9 mm
80 A 2.1 lb/h
0.95 kg/h
96 %
.045 in.
1.2 mm
250 A 7.6 lb/h
3.45 kg/h
96 %
.030 in.
0.8 mm
75 A 1.9 lb/h
0.86 kg/h
96 %
1/16 in.
1.6 mm
350 A 11.0 lb/h
6.21 kg/h
96 %
.035 in.
0.9 mm
150 A 4.1 lb/h
1.86 kg/h
96 %

Deposition Data

100% CO2
Diameter Current Deposition Rate Efficiency (%)
.045 in.
1.2 mm
250 A 7.4 lb/h
3.36 kg/h
93 %
1/16 in.
1.6 mm
350 A 10.7 lb/h
4.85 kg/h
93 %
.035 in.
0.9 mm
150 A 4.0 lb/h
1.81 kg/h
93 %
.045 in.
1.2 mm
125 A 2.7 lb/h
1.22 kg/h
93 %
.045 in.
1.2 mm
300 A 9.7 lb/h
4.40 kg/h
93 %
1/16 in.
1.6 mm
400 A 13.3 lb/h
6.03 kg/h
93 %
.035 in.
0.9 mm
200 A 5.9 lb/h
2.68 kg/h
93 %
.045 in.
1.2 mm
150 A 3.4 lb/h
1.54 kg/h
93 %
.045 in.
1.2 mm
350 A 12.5 lb/h
5.67 kg/h
93 %
1/16 in.
1.6 mm
450 A 16.5 lb/h
7.48 kg/h
93 %
1/16 in.
1.6 mm
250 A 6.2 lb/h
2.81 kg/h
93 %
1/16 in.
1.6 mm
275 A 7.3 lb/h
3.31 kg/h
93 %
1/16 in.
1.6 mm
300 A 8.5 lb/h
3.86 kg/h
93 %
.035 in.
0.9 mm
250 A 8.6 lb/h
3.90 kg/h
93 %
.045 in.
1.2 mm
200 A 5.3 lb/h
2.40 kg/h
93 %
.035 in.
0.9 mm
100 A 2.6 lb/h
1.18 kg/h
93 %
.045 in.
1.2 mm
100 A 1.9 lb/h
0.86 kg/h
93 %
.035 in.
0.9 mm
80 A 2.0 lb/h
0.91 kg/h
93 %

Approvals: ABS; AWS A5.18: ER70S-6 H4; CWB; CAN/CSA-ISO14341,B-G 49A 3C G6 (ER49S-6); CWB; CSA W48; LR; 3S, 3YS (H15); MIL-E-23765/1; MIL-70S-6
Classifications: ASME SFA-A5.18; ER70S-6; AWS A5.18; ER70S-6 H4