SPOOLARC 86

SPOOLARC 86

Spoolarc 86 is a copper-coated solid wire containing high levels of manganese and silicon. Spoolarc 86 is suitable for many carbon steel welding applications using the MIG/Gas Metal Arc Welding (GMAW) process. The high levels of deoxidizers in Spoolarc 86 provide excellent tolerance of rust and mill scale. The high levels of manganese and silicon also provide excellent wetting action and a highly fluid weld puddle. Shielding gas choices for Spoolarc 86 in the GMAW mode are 100% carbon dioxide, argon/carbon dioxide mixtures, argon/oxygen mixtures, and other argon based mixed gas blends. Spoolarc 86 excels in HVAC duct work, heavy equipment fabrication, structural, and other general steel fabrication.

Where To Buy


Industries

  • Automotive
  • Mobile Equipment
  • Industrial and General Fabrication
  • Ship/Barge Building

Welding Process

  • Welding-SAW - Submerged Arc Welding
  • Welding-GMAW (MIG/MAG - Metal Inert Gas / Metal Active Gas)
  • Welding-GTAW (TIG - Tungsten Inert Gas )

Specifications


Typical Tensile Properties

90% Ar - 10% CO2
Condition Elongation Tensile Strength Yield Strength
As Welded 29 % 86 ksi 73 ksi

Typical Charpy V-Notch Properties

90% Ar - 10% CO2
Condition Impact Value Testing Temperature
As Welded 96 ft-lb -50 °F
As Welded 91 ft-lb -40 °F
As Welded 115 ft-lb -20 °F

Typical Weld Metal Analysis %

ELEMENTVALUES
PMnMoCuSCSiNiCr
0.008 %1.51 %0.01 %0.11 %0.01 %0.08 %0.85 %0.01 %0.02 %

Approvals: ABS; AWS A5.18: ER70S-6 H4; CWB; CAN/CSA-ISO14341,B-G 49A 3C G6 (ER49S-6); CWB; CSA W48; LR; 3S, 3YS (H15); MIL-E-23765/1; MIL-70S-6
Classifications: ASME SFA-A5.18; ER70S-6; AWS A5.18; ER70S-6 H4