This site uses cookies and other tracking technologies to provide you with our services, enhance the performance and functionality of our services, analyze the use of our products and services, and assist with our advertising and marketing efforts.

Cookie Policy   Privacy Notice

Previous Next

ESAB

SPOOLARC 82

SPOOLARC 82

Spoolarc 82 is a premium quality, general purpose MIG wire subjected to stringent quality control procedures required for certification to Military, Lloyds, and ABS specifications. Spoolarc 82 is recommended for pressure vessel and pipe fabrication, HVAC duct work, and general carbon steel structural welding.

Where To Buy


Industries

  • Automotive
  • Industrial and General Fabrication
  • Pipeline
  • Mobile Equipment

Welding Process

  • Welding-GMAW (MIG/MAG - Metal Inert Gas / Metal Active Gas)
  • Welding-GTAW (TIG - Tungsten Inert Gas )

Specifications


Typical Tensile Properties

100% CO2
Condition Elongation Tensile Strength Yield Strength
As Welded 28 % 73 ksi 60 ksi
98% Ar - 2% O2
Condition Elongation Tensile Strength Yield Strength
As Welded 28 % 76 ksi 62 ksi

Typical Charpy V-Notch Properties

98% Ar - 2% O2
Condition Impact Value Testing Temperature
As Welded 83 ft-lb -20 °F
100% CO2
Condition Impact Value Testing Temperature
As Welded 75 ft-lb -20 °F

Typical Weld Metal Analysis %

ELEMENTVALUES
PMnMoCuSCVSiNiCr
0.011 %1.18 %0.01 %0.16 %0.007 %0.09 %0.004 %0.58 %0.02 %0.03 %

Approvals: ABS; AWS A5.18: ER70S-3 H4; CWB CSA W48; CAN/CSA-ISO14341,B-G 49A 2C G3 (ER49S-3); MIL-E-23765/1 MIL-70S-3
Classifications: AWS A5.18; ER70S-3 H4