This site uses cookies and other tracking technologies to provide you with our services, enhance the performance and functionality of our services, analyze the use of our products and services, and assist with our advertising and marketing efforts.

Cookie Policy   Privacy Notice

Previous Next

ESAB

SPOOLARC 29S

SPOOLARC 29S

Spoolarc 29S is a general purpose copper-coated solid wire suitable for many carbon steel welding applications using the MIG/Gas Metal Arc Welding (GMAW). Spoolarc 29S contains moderate amounts of manganese and silicon to provide sufficient deoxidation over light mill scale. Shielding gas choices for Spoolarc 29S in the GMAW mode are 100% carbon dioxide, argon/carbon dioxide mixtures, argon/oxygen mixtures, and other argon based mixed gas blends. Spoolarc 29S is used in a wide variety of applications including heavy equipment, automotive parts, railcars, agricultural equipment, and sheet metal welding.

Where To Buy


Industries

  • Mobile Equipment
  • Industrial and General Fabrication
  • Civil Construction
  • Automotive

Welding Process

  • Welding-GMAW (MIG/MAG - Metal Inert Gas / Metal Active Gas)

Specifications


Typical Tensile Properties

90% Ar - 10% CO2
Condition Elongation Tensile Strength Yield Strength
As Welded 22 % 85 ksi 72 ksi
75% Ar - 25% CO2
Condition Elongation Tensile Strength Yield Strength
As Welded 21 % 85 ksi 71 ksi

Typical Charpy V-Notch Properties

90% Ar - 10% CO2
Condition Impact Value Testing Temperature
As Welded 65 ft-lb -50 °F
As Welded 84 ft-lb -40 °F
As Welded 96 ft-lb -20 °F
75% Ar - 25% CO2
Condition Impact Value Testing Temperature
As Welded 58 ft-lb -50 °F
As Welded 60 ft-lb -40 °F
As Welded 73 ft-lb -20 °F

Typical Weld Metal Analysis %

ELEMENTVALUES
PMnMoCuCSVSiNiCr
0.015 %1.18 %0.01 %0.04 %0.09 %0.007 %0.004 %0.54 %0.04 %0.04 %

Approvals: ABS; 3SA, 3YSA; CWB; CAN/CSA-ISO14341,B-G 49A 2C G3 (ER49S-3); CWB; CSA W48
Classifications: AWS A5.18; ER70S-3