SPOOLARC 65

Typical Tensile Properties

98% Ar - 2% O2
Condition Elongation Tensile Strength Yield Strength
As Welded 26 % 82 ksi 70 ksi
100% Ar
Condition Elongation Tensile Strength Yield Strength
As Welded 26 % 79 ksi 67 ksi

Typical Charpy V-Notch Properties

100% Ar
Condition Impact Value Testing Temperature
As Welded 35 ft-lb -20 °F
98% Ar - 2% O2
Condition Impact Value Testing Temperature
As Welded 45 ft-lb -20 °F

Typical Weld Metal Analysis %

ELEMENTVALUES
MnMoCAlCrPCuSTiVSiZrNi
1.14 %0.01 %0.06 %0.08 %0.06 %0.004 %0.10 %0.006 %0.10 %0.01 %0.50 %0.04 %0.03 %

Deposition Data

Spray Transfer
Diameter Current Deposition Rate Voltage Wire Feed Speed
.035 in.
0.9 mm
180 A 6.3 lb/h
2.9 kg/h
25 V 400 in./min
1016 cm/min
.035 in.
0.9 mm
197 A 7.1 lb/h
3.2 kg/h
26 V 450 in./min
1143 cm/min
.035 in.
0.9 mm
213 A 7.9 lb/h
3.6 kg/h
26 V 500 in./min
1270 cm/min
.035 in.
0.9 mm
230 A 8.7 lb/h
4.0 kg/h
27 V 550 in./min
1397 cm/min
1/16 in.
1.6 mm
290 A 9.1 lb/h
4.1 kg/h
26 V 180 in./min
457 cm/min
1/16 in.
1.6 mm
310 A 10.1 lb/h
4.6 kg/h
28 V 200 in./min
508 cm/min
1/16 in.
1.6 mm
340 A 11.6 lb/h
5.3 kg/h
31 V 230 in./min
584 cm/min
1/16 in.
1.6 mm
370 A 13.2 lb/h
6.0 kg/h
34 V 260 in./min
660 cm/min
1/16 in.
1.6 mm
390 A 14.2 lb/h
6.4 kg/h
36 V 280 in./min
711 cm/min
.045 in.
1.2 mm
260 A 7.9 lb/h
3.6 kg/h
25 V 300 in./min
762 cm/min
.045 in.
1.2 mm
280 A 9.2 lb/h
4.2 kg/h
26 V 350 in./min
889 cm/min
.045 in.
1.2 mm
300 A 10.5 lb/h
4.8 kg/h
28 V 400 in./min
1016 cm/min
.045 in.
1.2 mm
320 A 11.8 lb/h
5.4 kg/h
29 V 450 in./min
1143 cm/min
.045 in.
1.2 mm
340 A 13.1 lb/h
6.0 kg/h
30 V 500 in./min
1270 cm/min

Deposition Data

Short Arc Transfer
Diameter Current Deposition Rate Voltage Wire Feed Speed
.045 in.
1.2 mm
130 A 3.1 lb/h
1.4 kg/h
17 V 125 in./min
318 cm/min
.045 in.
1.2 mm
163 A 4.0 lb/h
1.8 kg/h
18 V 160 in./min
406 cm/min
.045 in.
1.2 mm
200 A 5.0 lb/h
2.3 kg/h
19 V 200 in./min
508 cm/min
.035 in.
0.9 mm
90 A 2.7 lb/h
1.2 kg/h
15 V 180 in./min
457 cm/min
.035 in.
0.9 mm
113 A 3.3 lb/h
1.5 kg/h
16 V 220 in./min
559 cm/min
.035 in.
0.9 mm
137 A 4.0 lb/h
1.8 kg/h
18 V 260 in./min
660 cm/min
.035 in.
0.9 mm
160 A 4.6 lb/h
2.1 kg/h
19 V 300 in./min
762 cm/min

Approvals: MIL-E-23765/1; 70S-2
Classifications: AWS A5.18; ER70S-2 H4