This site uses cookies and other tracking technologies to provide you with our services, enhance the performance and functionality of our services, analyze the use of our products and services, and assist with our advertising and marketing efforts.

Cookie Policy   Privacy Notice

Previous Next

ESAB

SPOOLARC 65

SPOOLARC 65

Spoolarc 65 is a triple deoxidized (Aluminum, Titanium, Zirconium) welding wire designed for welding over rust and mill scale. The less fluid weld puddle of Spoolarc 65 makes it easy to control when used out of position. Spoolarc 65 is the preferred wire for all position welding of small diameter pipe. It is available in forms suitable for MIG and TIG welding.

Where To Buy


Industries

  • Power Generation
  • Military Applications
  • Pipeline
  • Ship/Barge Building

Welding Process

  • Welding-GMAW (MIG/MAG - Metal Inert Gas / Metal Active Gas)

Specifications


Typical Tensile Properties

98% Ar - 2% O2
Condition Elongation Tensile Strength Yield Strength
As Welded 26 % 82 ksi 70 ksi
100% Ar
Condition Elongation Tensile Strength Yield Strength
As Welded 26 % 79 ksi 67 ksi

Typical Charpy V-Notch Properties

100% Ar
Condition Impact Value Testing Temperature
As Welded 35 ft-lb -20 °F
98% Ar - 2% O2
Condition Impact Value Testing Temperature
As Welded 45 ft-lb -20 °F

Typical Weld Metal Analysis %

ELEMENTVALUES
MnMoCAlCrPCuSTiVSiZrNi
1.14 %0.01 %0.06 %0.08 %0.06 %0.004 %0.10 %0.006 %0.10 %0.01 %0.50 %0.04 %0.03 %

Approvals: MIL-E-23765/1; 70S-2
Classifications: AWS A5.18; ER70S-2 H4

Approvals are based on factory location. Please contact ESAB for more information.