OXWELD 1539 Series

OXWELD 1539 Series

Unsurpassed for washing off rivet heads and then piercing rivet to facilitate removal. Each nozzle is equipped with a spud which produces a low-velocity oxygen-stream.

Where To Buy


Features

  • Hard drawn, electrolytic, tough pitch copper used in one-piece nozzles – withstands heat and wear – outlasts any copper alloy nozzle
  • Precise CNC controlled drilling process ensures consistency in performance and quality
  • One-piece tips have triple swaged interior – gas passages are mirror smooth with internal
  • angles rounded for non-turbulent, more efficient gas flow – clean, smooth cuts with minimal kerf
  • Preheat ports are closely spaced around cutting orifice for greater concentration of preheat flames
  • Long, parallel preheat passages permit re-dressing tips without affecting performance
  • One-piece tips are a single piece of solid copper– provide maximum cooling – recommended always for acetylene, and for other fuel gases when heat exposure is unusually severe
  • Two-piece tips – recommended for high efficiency with alternate fuels – solid copper, heavy-wall external sleeve and brass internal sections can be ordered separately to minimize replacement cost

Industries

  • Industrial and General Fabrication
  • Light Fabrication
  • Repair and Maintenance
  • Structural Steel Fabrication

Specifications

Fuel Specifications

65Z55

Gas Pressure - Cutting Oxygen 80-90 psig
Gas Pressure - Fuel Gas 5-7 psig

65Z50

Gas Pressure - Cutting Oxygen 50-60 psig
Gas Pressure - Fuel Gas 5-7 psig

Operating Specifications

65Z55

Tip Size 19 in.

65Z50

Tip Size 19 in.

Tip Specifications

Cleaning Drill Size Cutting 3/16
Cleaning Drill Size Preheat 62
Preheat Holes 10
Tip Size 19 in.
Cleaning Drill Size Cutting 3/16
Cleaning Drill Size Preheat 62
Preheat Holes 10
Tip Size 19 in.