Previous Next

ESAB

OXWELD 1567 Series

OXWELD 1567 Series

Genuine OXWELD two-piece alternate fuel gas cutting nozzles are now available in matching sets. Take the guess work out of choosing the correct external nozzle for the alternate fuel gas being used and internal nozzle size.

Add to shopping list


Features

  • Hard drawn, electrolytic, tough pitch copper used in one-piece nozzles – withstands heat and wear – outlasts any copper alloy nozzle
  • One-piece nozzle has triple swaged interior – gas passages are mirror smooth with internal angles rounded for non-turbulent, more efficient gas flow – clean, smooth cuts with minimal kerf
  • Preheat ports are closely spaced around cutting orifice for greater concentration of preheat flames
  • Hard drawn, electrolytic, tough pitch copper used in one-piece nozzles – withstands heat and wear – outlasts any copper alloy nozzle
  • One-piece nozzle has triple swaged interior – gas passages are mirror smooth with internal angles rounded for non-turbulent, more efficient gas flow – clean, smooth cuts with minimal kerf
  • Preheat ports are closely spaced around cutting orifice for greater concentration of preheat flames
  • Long, parallel preheat passages – permit re-dressing nozzle without affecting performance
  • One-piece nozzle is a single piece of solid copper – provides maximum cooling – recommended always for acetylene, and for other fuel gases when heat exposure is unusually severe
  • Two-piece nozzles – recommended for high efficiency with fuel gases other than acetylene – solid copper, heavy-wall external sleeve and brass internal sections can be ordered separately to minimize replacement cost
  • Conical seats – instant aligning provides tight seal, prevents leaks around nozzle nut

Industries

  • Industrial and General Fabrication
  • Light Fabrication
  • Repair and Maintenance
  • Structural Steel Fabrication

Specifications

Fuel Specifications

639615

Gas Pressure - Cutting Oxygen 40 psig
Gas Pressure - Fuel Gas 3-5 psig
Total Fuel Gas Consumption 5-10 cfh
Total Oxygen Consumption 45-65 cfh

639616

Gas Pressure - Cutting Oxygen 40 psig
Gas Pressure - Fuel Gas 3-5 psig
Total Fuel Gas Consumption 5-10 cfh
Total Oxygen Consumption 65-85 cfh

Operating Specifications

639615

Average Kerf Width .050 in.
Cutting Speed 20-25 in./min
Metal Thickness 1/4 in.
Tip Size 1/4 in.

639616

Average Kerf Width .065 in.
Cutting Speed 18-25 in./min
Metal Thickness 1/2 in.
Tip Size 1/2 in.

Tip Specifications

Cleaning Drill Size Cutting 69
Metal Thickness 1/4 in.
Natural Gas External Part Number 639322
Natural Gas Internal Part Number 639615
Natural Gas Set Part Number 0558005016
Preheat Holes 12
Propylene External Part Number 998277
Propylene High External Part Number 998557
Propylene High Internal Part Number 639615
Propylene High Set Part Number 0558005040
Propylene Internal Part Number 639615
Propylene Set Part Number 0558005028
Tip Size 1/4 in.
Cleaning Drill Size Cutting 65
Metal Thickness 1/2 in.
Natural Gas External Part Number 639322
Natural Gas Internal Part Number 639616
Natural Gas Set Part Number 0558005017
Preheat Holes 12
Propylene External Part Number 998277
Propylene High External Part Number 998557
Propylene High Internal Part Number 639616
Propylene High Set Part Number 0558005041
Propylene Internal Part Number 639616
Propylene Set Part Number 0558005029
Tip Size 1/2 in.
x
×

Find the Closest Distributor

x

Find the Closest Distributor

x

x

Loading..