Previous Next

ESAB

OXWELD 1564 Series

OXWELD 1564 Series

Heavy preheat for beveling of prime coated steels or bevels in excess of 45 deg. Heavy scrap cutting.

Add to shopping list


Features

  • Hard drawn, electrolytic, tough pitch copper used in one-piece nozzles – withstands heat and wear – outlasts any copper alloy nozzle
  • One-piece nozzle has triple swaged interior – gas passages are mirror smooth with internal angles rounded for non-turbulent, more efficient gas flow – clean, smooth cuts with minimal kerf
  • Preheat ports are closely spaced around cutting orifice for greater concentration of preheat flames
  • Hard drawn, electrolytic, tough pitch copper used in one-piece nozzles – withstands heat and wear – outlasts any copper alloy nozzle
  • One-piece nozzle has triple swaged interior – gas passages are mirror smooth with internal angles rounded for non-turbulent, more efficient gas flow – clean, smooth cuts with minimal kerf
  • Preheat ports are closely spaced around cutting orifice for greater concentration of preheat flames
  • Long, parallel preheat passages – permit re-dressing nozzle without affecting performance
  • One-piece nozzle is a single piece of solid copper – provides maximum cooling – recommended always for acetylene, and for other fuel gases when heat exposure is unusually severe
  • Two-piece nozzles – recommended for high efficiency with fuel gases other than acetylene – solid copper, heavy-wall external sleeve and brass internal sections can be ordered separately to minimize replacement cost
  • Conical seats – instant aligning provides tight seal, prevents leaks around nozzle nut

Industries

  • Industrial and General Fabrication
  • Light Fabrication
  • Repair and Maintenance
  • Structural Steel Fabrication

Specifications

Fuel Specifications

638983

Gas Pressure - Cutting Oxygen 20-25 psig
Gas Pressure - Preheat Oxygen 20-50 psig
Gas Pressure - Propylene 3-5 psig
Total Acetylene Consumption 3-4 cfh
Total Oxygen Consumption 55-60 cfh
Gas Pressure - Cutting Oxygen 30-35 psig
Gas Pressure - Preheat Oxygen 20-50 psig
Gas Pressure - Propylene 3-5 psig
Total Acetylene Consumption 4-5 cfh
Total Oxygen Consumption 70-80 cfh

Operating Specifications

638983

Average Kerf Width .050 in.
Cutting Speed 18-24 in./min
Metal Thickness 1/4 in.
Tip Size 1/2 in.
Average Kerf Width .065 in.
Cutting Speed 14-22 in./min
Metal Thickness 1/2 in.
Tip Size 1/2 in.

Tip Specifications

Cleaning Drill Size Cutting 60
Cleaning Drill Size Preheat 67
Metal Thickness 1/8-1/2 in.
Preheat Holes 8
Tip Size 1/2 in.
Cleaning Drill Size Cutting 53
Cleaning Drill Size Preheat 64
Metal Thickness 3/4 - 1-1/2 in.
Preheat Holes 8
Tip Size 1-1/2 in.