OXWELD 1502 Series

OXWELD 1502 Series

General Purpose. Medium Preheat, sufficient preheat for cutting dirty plate and for beveling.

Where To Buy


Features

  • Hard drawn, electrolytic, tough pitch copper used in one-piece nozzles – withstands heat and wear – outlasts any copper alloy nozzle
  • One-piece nozzle has triple swaged interior – gas passages are mirror smooth with internal angles rounded for non-turbulent, more efficient gas flow – clean, smooth cuts with minimal kerf
  • Preheat ports are closely spaced around cutting orifice for greater concentration of preheat flames
  • Hard drawn, electrolytic, tough pitch copper used in one-piece nozzles – withstands heat and wear – outlasts any copper alloy nozzle
  • One-piece nozzle has triple swaged interior – gas passages are mirror smooth with internal angles rounded for non-turbulent, more efficient gas flow – clean, smooth cuts with minimal kerf
  • Preheat ports are closely spaced around cutting orifice for greater concentration of preheat flames
  • Long, parallel preheat passages – permit re-dressing nozzle without affecting performance
  • One-piece nozzle is a single piece of solid copper – provides maximum cooling – recommended always for acetylene, and for other fuel gases when heat exposure is unusually severe
  • Two-piece nozzles – recommended for high efficiency with fuel gases other than acetylene – solid copper, heavy-wall external sleeve and brass internal sections can be ordered separately to minimize replacement cost
  • Conical seats – instant aligning provides tight seal, prevents leaks around nozzle nut

Industries

  • Industrial and General Fabrication
  • Repair and Maintenance
  • Structural Steel Fabrication
  • Light Fabrication

Specifications

Fuel Specifications

08Z67

Gas Pressure - Acetylene 5-7 psig
Gas Pressure - Cutting Oxygen 30-35 psig
Gas Pressure - Preheat Oxygen 20-25 psig
Total Acetylene Consumption 6-8 cfh
Total Oxygen Consumption 35-45 cfh

15Z17

Gas Pressure - Acetylene 5-7 psig
Gas Pressure - Cutting Oxygen 35-40 psig
Gas Pressure - Preheat Oxygen 20-25 psig
Total Acetylene Consumption 8-10 cfh
Total Oxygen Consumption 65-75 cfh

Operating Specifications

08Z67

Average Kerf Width .045 in.
Cutting Speed 17-25 in./min
Metal Thickness 1/4 in.
Tip Size 1/4 in.

15Z17

Average Kerf Width .065 in.
Cutting Speed 15-23 in./min
Metal Thickness 1/2 in.
Tip Size 1/2 in.

Tip Specifications

Cleaning Drill Size Cutting 68
Cleaning Drill Size Preheat 69
Metal Thickness 1/4 in.
Preheat Holes 6
Tip Size 1/4 in.
Cleaning Drill Size Cutting 60
Cleaning Drill Size Preheat 66
Metal Thickness 1/2 in.
Preheat Holes 6
Tip Size 1/2 in.